TiS2

    Our TiS2 crystals are stabilized in 1T semi-metallic phase and they are grown using two different techniques through chemical vapor transport (CVT) or flux zone growth (see description of these two methods below). These crystals are treated as gold standards in 2D materials field owing to perfected electronic behavior with guaranteed phase transition and semi-metallic responses. Our TiS2 crystals are notoriously known low impurity resistance (zero temperature resistance), high carrier mobility, extremely clean and sharp XRD peaks, and negligible amount of defects (see published results as well as CVT vs. Flux based methods below ). Our TiS2 crystals are large in size and ready for exfoliation without any preparation.

Properties of vdW TiS2 crystals

Sample sizeReaching to cm size 001 oriented crystals
Material propertiesSemimetal
Crystal structureTrigonal phase a=b=0.338 nm c=0.574 nm 
Degree of exfoliationVery easy to exfoliate
Production method

Flux zone growth no contaminations least grain boundary 

[Optional] CVT grown crystals halide contamination and more defected.

Other characteristics
  • High environmental stability
  • 99.9999% confirm purity on flux zone grown crystals
  • Easy to exfoliate
  • Ready to exfoliate
  • Excellent customer service and return policy

Growth method matters> Flux zone or CVT growth method

     Contamination of halides and point defects in layered crystals are well known cause for their reduced electronic mobility, reduced anisotropic response, poor e-h recombination, low-PL emission, and lower optical absorption. Flux zone technique is a halide free technique used for synthesizing truly semiconductor grade vdW crystals. This method distinguishes itself from chemical vapor transport (CVT) technique in the following regard: CVT is a quick (~2 weeks) growth method but exhibits poor crystalline quality and the defect concentration reaches to 1E11 to 1E12 cm-2 range. In contrast, flux method takes long (~3 months) growth time, but ensures slow crystallization for perfect atomic structuring, and impurity free crystal growth with defect concentration as low as 1E9 - 1E10 cm-2. During check out just state which type of growth process is preferred. Unless otherwise stated, 2Dsemiconductors ships Flux zone crystals as a default choice. 

其他服务:

  公司可以提供免费的机械剥离和转移技术


关于我们   新闻中心   更多信息   合作企业
关于我们
牧科愿景
牧科石墨烯
应用领域
  公司新闻
产品新闻
行业动态
  法律申明
诚聘英才
 
版权所有 南京牧科纳米科技有限公司

服务时间:周一至周日 08:30 — 20:00  全国订购及服务热线:025-66171690 18052095282
联系地址:南京市麒麟科技创新园康园路20号南京空间大数据产业基地B栋 苏ICP备15025922号-1

南京岩棉板 江苏岩棉板 南京生物质颗粒 催化剂装卸 南京网站设计采矿台车 液压台车  南京生物质颗粒燃料 南京模型公司 南京百度竞价托管代运营